  • logoImg.jpg

Polyurethane primer

This product is a two component acrylic polyurethane floor paint, consisting of A component (resin) and B component (curing agent) as solvent based coatings. It has low odor, good dryness, and strong sealing properties, belonging to the category of low viscosity and high permeability. It can effectively penetrate into the interior of the foundation and has strong adhesion to the ground foundation.

Details

1、 Product Introduction
This product is a two component acrylic polyurethane floor paint, consisting of A component (resin) and B component (curing agent) as solvent based coatings. It has low odor, good dryness, and strong sealing properties, belonging to the category of low viscosity and high permeability. It can effectively penetrate into the interior of the foundation and has strong adhesion to the ground foundation.
2、 Usage method
(1) Before use, component A (resin) should be thoroughly stirred with an explosion-proof mixer and stirred at high speed for 1-3 minutes
(2) A component (resin) and B component (curing agent) should be weighed using a standard measuring device according to the proportion indicated on the packaging label to ensure their accuracy. After mixing, they should not be mixed randomly to avoid affecting the curing effect of the material.
(3) Pour the mixed AB components and the prepared materials onto the floor. Professional construction workers will work according to the construction requirements to achieve the desired effect. Generally, roller coating and scraping method are used, but it must be evenly applied.
(4) For areas with poor ground foundation, it is necessary to apply multiple times to achieve sealing effect.
3、 Precautions:
(1) This product belongs to flammable chemicals. Please stay away from ignition sources and use explosion-proof motors for the mixer.
(2) This product should be stored in a cool and ventilated place and should not be exposed to the sun.
(3) Do not use this product at a temperature below 5 ℃ for construction, as low temperatures can affect the curing time.
(4) During the construction process, if materials are accidentally splashed into the eyes, they should be promptly rinsed with clean water and sent to the hospital for treatment.